CC BY 4.0 · Eur J Dent 2024; 18(02): 665-671
DOI: 10.1055/s-0043-1777044
Original Article

Osteogenic Differentiation and Proliferation of Apical Papilla Stem Cells Using Chitosan-Coated Nanohydroxyapatite and Bioactive Glass Nanoparticles

Sara Elshahat
1   Endodontic Department, Faculty of Dentistry, Ain Shams University, Cairo, Egypt
,
Abeer Abdelhakim Elgendy
1   Endodontic Department, Faculty of Dentistry, Ain Shams University, Cairo, Egypt
,
1   Endodontic Department, Faculty of Dentistry, Ain Shams University, Cairo, Egypt
2   Restorative Dental Sciences Department, College of Dentistry, Gulf Medical University, Ajman, UAE
› Author Affiliations

Abstract

Objective The aim of this study was to evaluate the osteogenic differentiation ability and proliferation of apical papilla stem cells (SCAPs) using chitosan-coated nanohydroxyapatite and bioactive glass nanoparticles.

Materials and Methods Hydroxyapatite, chitosan-coated nanohydroxyapatite, and bioactive glass 45S5 nanoparticles were prepared and characterized using a transmission electron microscope and X-ray diffraction. SCAPs were harvested from freshly extracted impacted wisdom teeth, cultured, and characterized using flow cytometric analysis. Tested nanomaterials were mixed and samples were classified into five equal groups as follows: negative control group: SCAP with Dulbecco's modified eagle's medium, positive control group: SCAP with inductive media, first experimental group: nanohydroxyapatite with SCAP, second experimental group: chitosan-coated nanohydroxyapatite with SCAP, third experimental group: bioactive glass nanoparticles with SCAP. Osteoblastic differentiation was assessed using an alkaline phosphatase (ALP) assay. Receptor activator of nuclear factor kappa beta ligand (RANKL) expression was evaluated using specific polyclonal antibodies by fluorescence microscope. The proliferation of SCAP was assessed using cell count and viability of trypan blue in addition to an 3-(4,5-dimethylthiazol-2-yl)-2,5-diphenyltetrazolium bromide (MTT) assay.

Results Isolated SCAP showed a nonhematopoietic origin. Chitosan-coated nanohydroxyapatite showed the highest ALP concentration followed by nanobioactive glass, nanohydroxyapatite, and negative control. Chitosan-coated nanohydroxyapatite showed the highest H score followed by nanobioactive glass, nanohydroxyapatite, and negative control in RANKL expression. Chitosan-coated nanohydroxyapatite showed the highest viable cell count.

Conclusion SCAP isolation is achievable from extracted fully impacted immature third molars. All tested biomaterials have the ability to induce osteogenic differentiation and proliferation of SCAP. Composite nanoparticle materials show better osteogenic differentiation and proliferation of SCAP than single nanoparticles.

Ethical Approval Statement

The research proposal was approved by the Faculty of Dentistry Ain Shams University ethical committee with approval number FDASU-Rec IM112105.




Publication History

Article published online:
05 March 2024

© 2024. The Author(s). This is an open access article published by Thieme under the terms of the Creative Commons Attribution License, permitting unrestricted use, distribution, and reproduction so long as the original work is properly cited. (https://creativecommons.org/licenses/by/4.0/)

Thieme Medical and Scientific Publishers Pvt. Ltd.
A-12, 2nd Floor, Sector 2, Noida-201301 UP, India

 
  • References

  • 1 Yan M, Wu J, Yu Y. et al. Mineral trioxide aggregate promotes the odonto/osteogenic differentiation and dentinogenesis of stem cells from apical papilla via nuclear factor kappa B signaling pathway. J Endod 2014; 40 (05) 640-647
  • 2 Sonoyama W, Liu Y, Yamaza T. et al. Characterization of the apical papilla and its residing stem cells from human immature permanent teeth: a pilot study. J Endod 2008; 34 (02) 166-171
  • 3 Nada OA, El Backly RM. Stem cells from the apical papilla (SCAP) as a tool for endogenous tissue regeneration. Front Bioeng Biotechnol 2018; 6 (July): 103
  • 4 Sun JY, Yang YS, Zhong J, Greenspan DC. The effect of the ionic products of bioglass dissolution on human osteoblasts growth cycle in vitro. J Tissue Eng Regen Med 2007; 1 (04) 281-286
  • 5 Xynos ID, Hukkanen MV, Batten JJ, Buttery LD, Hench LL, Polak JM. Bioglass 45S5 stimulates osteoblast turnover and enhances bone formation In vitro: implications and applications for bone tissue engineering. Calcif Tissue Int 2000; 67 (04) 321-329
  • 6 MačKović M, Hoppe A, Detsch R. et al Bioactive glass (type 45S5) nanoparticles: in vitro reactivity on nanoscale and biocompatibility. J Nanopart Res 2012; 14: 966
  • 7 El-Gendy R, Yang XB, Newby PJ, Boccaccini AR, Kirkham J. Osteogenic differentiation of human dental pulp stromal cells on 45S5 Bioglass® based scaffolds in vitro and in vivo. Tissue Eng Part A 2013; 19 (5-6): 707-715
  • 8 Yousefi AM, Oudadesse H, Akbarzadeh R, Wers E, Lucas-Girot A. Physical and biological characteristics of nanohydroxyapatite and bioactive glasses used for bone tissue engineering. Nanotechnol Rev 2014; 3 (06) 527-552
  • 9 Ratih DN, Mulyawati E, Santi RK, Kristanti Y. Antibacterial and cytotoxicity of root canal sealer with the addition of chitosan nanoparticle at various concentrations. Eur J Dent 2023; 17 (02) 398-402
  • 10 Putranto AW, Suprastiwi E, Meidyawati R, Agusnar H. Characterization of novel cement-based carboxymethyl chitosan/amorphous calcium phosphate. Eur J Dent 2022; 16 (04) 809-814
  • 11 Torres-Rosas R, Torres-Gómez N, Moreno-Rodríguez A, García-Contreras R, Argueta-Figueroa L. Anti-inflammatory and antibacterial activity of the chitosan/chlorhexidine gel commercial preparation for postexodontia treatment: an in vitro study. Eur J Dent 2020; 14 (03) 397-403
  • 12 Boudemagh D, Venturini P, Fleutot S, Cleymand F. Elaboration of Hydroxyapatite Nanoparticles and Chitosan/Hydroxyapatite Composites: A Present Status [Internet]. Vol. 76, Polymer Bulletin. Berlin:: Springer;; 2019: 2621-2653 p.
  • 13 Vafa E, Bazargan-Lari R, Bahrololoom ME. Synthesis of 45S5 bioactive glass-ceramic using the sol-gel method, catalyzed by low concentration acetic acid extracted from homemade vinegar. J Mater Res Technol 2021; 10: 1427-1436
  • 14 Cengiz B, Gokce Y, Yildiz N, Aktas Z, Calimli A. Synthesis and characterization of hydroxyapatite nanoparticles. Colloids Surf A Physicochem Eng Asp 2008; 322 (1–3) 29-33
  • 15 Nikpour MR, Rabiee SM, Jahanshahi M. Synthesis and characterization of hydroxyapatite/chitosan nanocomposite materials for medical engineering applications. Compos, Part B Eng 2012; 43 (04) 1881-1886
  • 16 Vuong Bùi X. Bioactive ceramic powder prepared using a new sol-gel process. Process Appl Ceram 2017; 11 (02) 87-92
  • 17 El shahat S, Elgendy AA, Elsewify T. Characterization of human stem cells of the apical papilla. Ain Shams Dental Journal 2021; 24: 17-23
  • 18 Chueh LH, Ho YC, Kuo TC, Lai WH, Chen YHM, Chiang CP. Regenerative endodontic treatment for necrotic immature permanent teeth. J Endod 2009; 35 (02) 160-164
  • 19 Miller AA, Takimoto K, Wealleans J, Diogenes A. Effect of 3 bioceramic materials on stem cells of the apical papilla proliferation and differentiation using a dentin disk model. J Endod 2018; 44 (04) 599-603
  • 20 Lei G, Yan M, Wang Z. et al. Dentinogenic capacity: immature root papilla stem cells versus mature root pulp stem cells. Biol Cell 2011; 103 (04) 185-196
  • 21 Li J, Yan M, Wang Z. et al Effects of canonical NF-κB signaling pathway on the proliferation and odonto/osteogenic differentiation of human stem cells from apical papilla. Biomed Res Int 2014; 2014: 319651
  • 22 Gong W, Huang Z, Dong Y. et al. Ionic extraction of a novel nano-sized bioactive glass enhances differentiation and mineralization of human dental pulp cells. J Endod 2014; 40 (01) 83-88
  • 23 Gough JE, Jones JR, Hench LL. Nodule formation and mineralisation of human primary osteoblasts cultured on a porous bioactive glass scaffold. Biomaterials 2004; 25 (11) 2039-2046
  • 24 Gholami S, Labbaf S, Houreh AB, Ting HK, Jones JR, Nasr Esfahani MH. Long term effects of bioactive glass particulates on dental pulp stem cells in vitro. Biomed Glas 2017; 3 (01) 96-103
  • 25 Yang X, Li Y, Liu X, Zhang R, Feng Q. In vitro uptake of hydroxyapatite nanoparticles and their effect on osteogenic differentiation of human mesenchymal stem cells. Stem Cells Int 2018; 2018: 2036176
  • 26 Houreh AB, Labbaf S, Ting HK, Ejeian F, Jones JR, Esfahani MHN. Influence of calcium and phosphorus release from bioactive glasses on viability and differentiation of dental pulp stem cells. J Mater Sci 2017; 52 (15) 8928-8941
  • 27 Amir LR, Suniarti DF, Utami S, Abbas B. Chitosan as a potential osteogenic factor compared with dexamethasone in cultured macaque dental pulp stromal cells. Cell Tissue Res 2014; 358 (02) 407-415
  • 28 Piccinini F, Tesei A, Arienti C, Bevilacqua A. Cell counting and viability assessment of 2D and 3D cell cultures: expected reliability of the trypan blue assay. Biol Proced Online 2017; 19 (01) 8
  • 29 Di Nardo P. et al. Adult Stem Cells Methods and Protocols. New York, NY: Springer Science + Business Media LLC; 2017: 194
  • 30 Plumb JA. Cell Sensitivity Assays: The MTT Assay. Langdon S.P.. (eds), Cancer Cell Culture. Methods in Molecular Medicine. Totowa, NJ: Humana Press; 2004
  • 31 Gomes-Cornélio AL, Rodrigues EM, Salles LP. et al. Bioactivity of MTA Plus, Biodentine and an experimental calcium silicate-based cement on human osteoblast-like cells. Int Endod J 2017; 50 (01) 39-47
  • 32 Reilly GC, Radin S, Chen AT, Ducheyne P. Differential alkaline phosphatase responses of rat and human bone marrow derived mesenchymal stem cells to 45S5 bioactive glass. Biomaterials 2007; 28 (28) 4091-4097
  • 33 Ryu W-S. Diagnosis and methods. Mol Virol Hum Pathog Viruses 2017; 47-62
  • 34 Magri AMP, Fernandes KR, Ueno FR. et al. Osteoconductive properties of two different bioactive glass forms (powder and fiber) combined with collagen. Appl Surf Sci 2017; 423: 557-565
  • 35 Gabbai-Armelin PR, Souza MT, Kido HW. et al. Effect of a new bioactive fibrous glassy scaffold on bone repair. J Mater Sci Mater Med 2015; 26 (05) 177
  • 36 Kang J, Fan W, Deng Q, He H, Huang F. Stem cells from the apical papilla: a promising source for stem cell-based therapy. BioMed Res Int 2019; 2019: 6104738
  • 37 Kong L, Gao Y, Lu G, Gong Y, Zhao N, Zhang X. A study on the bioactivity of chitosan/nano-hydroxyapatite composite scaffolds for bone tissue engineering. Eur Polym J 2006; 42 (12) 3171-3179
  • 38 Hosseinzade M, Soflou RK, Valian A, Nojehdehian H. Physicochemical properties of MTA, CEM, hydroxyapatite and nano hydroxyapatite-chitosan dental cements. Biomed Res 2016; 27 (02) 442-448
  • 39 Ge S, Zhao N, Wang L. et al. Bone repair by periodontal ligament stem cellseeded nanohydroxyapatite-chitosan scaffold. Int J Nanomedicine 2012; 7: 5405-5414
  • 40 Matsunaga T, Yanagiguchi K, Yamada S, Ohara N, Ikeda T, Hayashi Y. Chitosan monomer promotes tissue regeneration on dental pulp wounds. J Biomed Mater Res A 2006; 76 (04) 711-720
  • 41 Dash M, Chiellini F, Ottenbrite RM, Chiellini E. Chitosan - a versatile semi-synthetic polymer in biomedical applications. Prog Polym Sci 2011; 36 (08) 981-1014
  • 42 Lieder R. Chitosan and chitosan derivatives in tissue engineering and stem cell biology. PhD thesis, Reykjavik Univ. 2013. ;(January):141
  • 43 Tondnevis F, Ketabi M, Fekrazad R, Sadeghi A, Abolhasani MM. Using chitosan besides nano hydroxyapatite and fluorohydroxyapatite boost dental pulp stem cell proliferation. J Biomim Biomater Biomed Eng 2019; 42: 39-50
  • 44 Wang S, Huang G, Dong Y. Directional migration and odontogenic differentiation of bone marrow stem cells induced by dentin coated with nanobioactive glass. J Endod 2020; 46 (02) 216-223